Sign In | Join Free | My benadorassociates.com
China Beijing Tonghe Testing Machine Co., ltd logo
Beijing Tonghe Testing Machine Co., ltd
WE OFFER ONLY WHAT SUITS YOU BEST!
Verified Supplier

2 Years

Home > Differential Scanning Calorimeter >

High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model

Beijing Tonghe Testing Machine Co., ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model

Brand Name : JINHAIHU

Model Number : DSC-800B

Certification : ISO9001

Place of Origin : BEIJING, CHINA

MOQ : 1 set

Supply Ability : 20 sets per month

Delivery Time : 7-15 working days

Packaging Details : Conventional export wooden crates

Payment Terms : L/C,D/A,D/P,T/T,Western Union,MoneyGram

Product name : DSC-800B Differential Scanning Calorimeter/Oxidation induction time

Temperature Range : Room temperature to 800 ℃

Temperature resolution : 0.1 ℃

Heating rate : 0.1 ~ 80 ℃ / min

DSC range : 0~±200mW

Gas flow : 0-200mL/min

DSC sensitivity : 0.1 mW

Gas pressure : 0.2MPa

Contact Now

DSC-800B Differential Scanning Calorimeter/Oxidation induction time


Technical feature:

1.Industrial-grade widescreen touch structure with comprehensive display: set temperature, sample temperature, oxygen flow rate, nitrogen flow, differential thermal signals, various switch states, and flow zero indication.
2.USB communication interface with high universality, reliable non-interruptive connection, and support for recovery function.
3.Compact furnace design with infinitely adjustable cooling rate.
4.Enhanced installation process using mechanical fixing to completely prevent internal colloid from contaminating differential thermal signals.
5.Dual temperature probes ensure repeatable sample temperature measurement at specified heights.
6.One temperature sensor on the furnace wall enables PID control of furnace temperature, but thermal inertia causes sample temperature deviation (varying by season). Single-probe measurement leads to significant errors in both thermal and temperature signals. The instrument installs a bottom-mounted probe to measure true sample temperature, using proprietary control technology to adjust furnace wall temperature to the set value.
7.Digital gas mass flowmeter for automatic two-way atmosphere switching with fast response and short stabilization time.
8.Calibrated with standard samples for easy customer adjustment of temperature coefficients.
9.Software adapts to all screen resolutions, automatically optimizing curve display based on screen size. Compatible with laptops/desktops, supporting Win2000, XP, VISTA, Windows 7, etc.
10.User-programmable procedures enable fully automated measurements. Dozens of commands allow flexible combination and saving, simplifying complex operations to one-key functions.

Technical parameter:

Temperature range room temperature ~800℃
Temperature resolution 0.01℃
Heating rate 0.1~80℃/min ;
Temperature control mode rise in temperature, constant temperature (Programs control automatically)
DSC range 0~±200mW
DSC resolution 0.01mW
DSC sensitivity 0.1mW
Working power supply AC 220V 50Hz or custom-made
Atmosphere control of gas nitrogen ;oxygen (instrument changes automatically)
Gas flow 0-200mL/min
Gas pressure 0.2MPa
Accuracy of gas flow 0.2mL/min
Matching crucible Alumina crucible Φ6.7*3mm
Parameter standard equipped with standard material(indium ,tin, zinc) the user can correct the temperature and enthalpy
Data interface standard USB interface
Display mode 24bit color 7 inch LED touch screen display
Output mode computer and printer

Standard Configuration list:

Model quantity unit note
DSC 1 SET

Fit Model:

DSC-500A

DSC-500B

DSC-800B

DSC-500BL

DSC-1150B


Aluminum crucible 300 PCS
Standard test samples (indium, tin, and zinc) 1 Part
power wire and USB 1 PCS
Software CD 1 PCS
tweezers 1 PCS
Medicine spoon 1 PCS
Custom valve connector 2 PCS
Oxygen and nitrogen gas duct 5 Meter
quick coupling 2 PCS
Soft dog 1 PCS
Fusing glass fuse 4 PCS


Package:

Product weight:23 kg

product dimensions: length 45 cm * 30 cm * 27 cm

aluminum box size: 41 cm * 30 cm * 53 cm

paper box outside wrapping paper box size: 50 cm * 60 cm* 39 cm



High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model

High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model

High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model

High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model


Product Tags:

High Sensitivity Differential Scanning Calorimetry

      

High Sensitivity DSC Equipment

      

DSC Calorimeter DSC-800B

      
Quality High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model for sale

High Sensitivity Differential Scanning Calorimetry Machine DSC-800B Model Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Beijing Tonghe Testing Machine Co., ltd
*Subject:
*Message:
Characters Remaining: (0/3000)